Ku rakibidda birta waxay inta badan soo saartaa cillado kala duwan oo wax-soo-saarka.Hadda Shijiazhuang donghuan malleable technology birta co., Ltd kuu sheego sida looga hortago cilladaha sida ayaa had iyo jeer dhibaato in saarayaasha tuuro ka walaacsan yihiin.
Aqoon-is-weydaarsiga wax-soo-saarku wuxuu inta badan adeegsadaa habka shubista ciid-cagaarka ee dhaqameed si loo soo saaro shubista birta.Wax soo saarka muddada dheer, waxaa la ogaadaa in cilladaha soo socdaa ay inta badan ku dhacaan birta wax lagu shubo, sida godadka ciidda, ciidda dhegta, daloolada, godadka, ciidda isku darka iyo nabarrada, bararka, ciidda kuwan.
1. Tallaabooyinka ka hortagga trachoma:
(1) Si adag u xakamee waxqabadka ciidda wax ka beddelidda;
(2) Kahor intaadan xidhin sanduuqa, xalli ciidda sabaynaysa dusha caaryada caaryada ah iyo xudunta cammuudda si fiican oo si adag u xidh sanduuqa;
(3) Deji software ku habboon oo wax ku ool ah nidaamka shubista;
(4) lakabka sare ee koobka shubaya waa inuu ahaadaa mid siman oo nadiif ah, mana jiri karto ciid sabaynaysa.
2. Tallaabooyinka ka hortagga ciidda ku dheggan
(1) Isticmaal ciid leh iska caabbinta dabka sare;
(2) Si dhexdhexaad ah u yaree heerkulka shubista oo kordhi heerka shubista;
(3) Cufnaanta caaryada ciidda waa in ay ahaataa mid sare (guud ahaan in ka badan 85) oo si fiican loo siman yahay;
(4) Dooro dahaarka dhismaha ee aan dillaacin heerkulka sare oo aan gelin godadka dhalaalay.
Ku soo dhawoow inaad kala tashato shirkadeena dhibaatooyinka kala duwan ee kabka.
Waqtiga boostada: Agoosto-01-2022